LI Suan. NEN REPAIR METHOD OF BEARING PAD DAMAGE FOR A BALL TUBE MILL[J]. Thermal power generation, 2002, (5): 50-51. DOI: 10.19666/j.rlfd.2002.05.016.
一种钢球磨煤机轴瓦损伤修复新方法
摘要
通过分析广州发电厂 2号锅炉乙磨煤机出口轴瓦损伤情况
采用不顶大罐
“灌油慢转打磨法”进行修复。修复后经过近 7年的运行
无异常情况
说明修复措施简单有效
Abstract
Through analysing the bearing pad damage of ball tube mill No.2 belonging to boiler No.2 at Guangzhou Power Plant
a new repair method
namely oil-pouring low speed grinding method without lifting the big canister
was selected. After repairing
there was no abnormality occurred in long-term operation of about seven years
it is clear that the new repair method being simple and correct.