1. 电工材料电气绝缘全国重点实验室(西安交通大学),西安,710049
2. 王青于,1991—,女,博士,副教授,主要从事超/特高压交、直流套管绝缘结构优化设计、电接触特性及多物理场数值计算方法等方面的研究工作,E-mail:
收稿:2026-06-30,
纸质出版:2026
移动端阅览
谢韬, 刘则希, 王青于, 等. 换流变阀侧套管电连接部件静态连接特性与故障早期诱因[J]. 高电压技术, 2026,52(6):2778-2788.
XIE Tao, LIU Zexi, WANG Qingyu, et al. 换流变阀侧套管电连接部件静态连接特性与故障早期诱因[J]. 2026, 52(6): 2778-2788.
谢韬, 刘则希, 王青于, 等. 换流变阀侧套管电连接部件静态连接特性与故障早期诱因[J]. 高电压技术, 2026,52(6):2778-2788. DOI: 10.13336/j.1003-6520.hve.20251653.
XIE Tao, LIU Zexi, WANG Qingyu, et al. 换流变阀侧套管电连接部件静态连接特性与故障早期诱因[J]. 2026, 52(6): 2778-2788. DOI: 10.13336/j.1003-6520.hve.20251653.
随着电网输送能力的提升,套管等电力设备承载着更高的电压和更大的电流,触指类电连接部件面临着更加严苛的运行挑战。为研究电连接部件故障早期诱因,以换流变阀侧套管电连接部件为研究对象,开展触指静态通流试验,并构建三维精细化模型进行电-热耦合的多物理场计算,获得触指的温度场分布。基于静态通流试验从表面形貌、微观结构和化学腐蚀三方面开展触指在变压器油环境下的故障早期诱因分析。研究结果表明,油温为80 ℃时且单片触指通过满载电流60 A时,其接触区域温度可达120.6 ℃。触指在接触初期电阻波动较大,运行5 d后接触电阻趋于稳定,在均值159.71 μΩ附近波动,波动幅值小于1.6%。在触指与导体的接触表面观测到了微焊接现象,并通过表征接触区域微观组织结构发生的重结晶行为,论证了触点超温现象,解释了微焊接行为的发生。触指表面有明显的腐蚀痕迹,腐蚀产物以硫化物为主,且铜材料更易与油中腐蚀性硫化物反应,腐蚀产物会发生迁移并在镀银表面附着。该研究结果可为电连接部件故障早期诱因研究和表带触指的国产化设计提供理论依据。
With the enhancement of the power grid's transmission capacity
power devices such as bushings are subjected to higher voltages and larger currents
posing more stringent operational challenges to electrical connection components. To investigate the early causes of failures in electrical connection components
this paper focuses on the electrical connection components of the valve-side bushings in converter transformers
conducting static current-carrying tests on contactor and constructing a three-dimensional refined model for electro-thermal coupling multi-physical field calculations to obtain the temperature field distribution of the contactor. Based on static current-carrying tests
an analysis of the early failure causes of contactors in transformer oil environments is conducted from following three aspects: surface morphology
microstructure
and chemical corrosion. The research results indicate that
when the oil temperature is 80 ℃ and a single contactor carries a full-load current of 60 A
the temperature in the contact area can reach 120.6 ℃. During the initial contact phase
the resistance of the contactor exhibits significant fluctuations. After five days of operation
the contact resistance is stabilized
oscillating around a mean value of 159.71 μΩ with an amplitude of less than 1.6%. Micro-welding phenomena can be observed on the contact surface between the contactor and the conductor. Through the characterization of the recrystallization behavior in the microstructure of the contact area
the phenomenon of contact overheating is demonstrated
explaining the occurrence of micro-welding. Significant corrosion marks can be observed on the surface of the contactor
with sulfides being the primary corrosion products. Copper materials are more prone to react with corrosive sulfides in oil
leading to the migration and attachment of corrosion products on the silver-plated surface. The findings of this study can provide a theoretical basis for research on the early failure causes of electrical connection components and the domestic design of strap-type contactors.