TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF
热力发电2011年40卷第3期 页码:78-80
作者机构:
华能德州电厂
作者简介:
基金信息:
DOI:
中图分类号:TK228
纸质出版:2011
稿件说明:
移动端阅览
李庆义. 锅炉尾部受热面管磨损及处理方法[J]. 热力发电, 2011,40(3):78-80.
LI Qingyi Huaneng Dezhou Power Plant. TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF[J]. Thermal power generation, 2011, 40(3): 78-80.
LI Qingyi Huaneng Dezhou Power Plant. TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF[J]. Thermal power generation, 2011, 40(3): 78-80.DOI:
锅炉尾部受热面管磨损及处理方法
摘要
某电厂锅炉尾部受热面管子多次出现磨损泄漏
分析其原因是锅炉尾部受热面管排布置不合理
使烟气流速增加
并转向冲刷低温再热器和低温过热器管排所致。对此
提出了在低温过热器左右1~3排各9根增加防磨套
左右1~6排低温过热器与入口联箱和侧包墙过热器出口联箱用耐火水泥敷设防磨等处理措施。
Abstract
Abrasion leakages have frequently occurred on tubes of the heat recovery surface in tail section of boilers in one power plant.It is believed from analysis that the main cause is due to unreasonable arrangement of tube rows on the heat recovery surface in tail section of boilers
making the flue gas to increase flow velocity and change direction to scour the low-temperature reheater and low-temperature superheater.For this
some measures have been put forward as in the following:1) installing wear-resisting casings on nine tubes in 1~3 pipe rows at the left and right side of the low-temperature superheater;2) laying coatings of refractory cement on 1~6 pipe rows at left and right side of the low-temperature superheater
as well as on inlet header and outlet header of the steam cooled wall.