TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF
|更新时间:2025-09-28
|
TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF
Thermal Power GenerationVol. 40, Issue 3, Pages: 78-80(2011)
作者机构:
华能德州电厂
作者简介:
基金信息:
DOI:
CLC:TK228
Published:2011
稿件说明:
移动端阅览
LI Qingyi Huaneng Dezhou Power Plant. TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF[J]. Thermal power generation, 2011, 40(3): 78-80.
DOI:
LI Qingyi Huaneng Dezhou Power Plant. TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF[J]. Thermal power generation, 2011, 40(3): 78-80.DOI:
TUBE ABRASION ON HEAT RECOVERY SURFACE IN TAIL SECTION OF BOILERS AND DISPOSAL METHOD THEREOF
摘要
某电厂锅炉尾部受热面管子多次出现磨损泄漏
分析其原因是锅炉尾部受热面管排布置不合理
使烟气流速增加
并转向冲刷低温再热器和低温过热器管排所致。对此
提出了在低温过热器左右1~3排各9根增加防磨套
左右1~6排低温过热器与入口联箱和侧包墙过热器出口联箱用耐火水泥敷设防磨等处理措施。
Abstract
Abrasion leakages have frequently occurred on tubes of the heat recovery surface in tail section of boilers in one power plant.It is believed from analysis that the main cause is due to unreasonable arrangement of tube rows on the heat recovery surface in tail section of boilers
making the flue gas to increase flow velocity and change direction to scour the low-temperature reheater and low-temperature superheater.For this
some measures have been put forward as in the following:1) installing wear-resisting casings on nine tubes in 1~3 pipe rows at the left and right side of the low-temperature superheater;2) laying coatings of refractory cement on 1~6 pipe rows at left and right side of the low-temperature superheater
as well as on inlet header and outlet header of the steam cooled wall.