Regeneration of K poisoned commercial SCR catalyst by acid washing
|更新时间:2025-09-28
|
Regeneration of K poisoned commercial SCR catalyst by acid washing
Thermal Power GenerationVol. 43, Issue 7, Pages: 104-109(2014)
作者机构:
1. 广东电网公司电力科学研究院
2. 华南理工大学环境与能源学院
3. 广东省大气环境与污染控制重点实验室
作者简介:
基金信息:
DOI:
CLC:X773;O643.36
Published:2014
稿件说明:
移动端阅览
PAN Siwei, CHENG Hua, WEI Zhengle, et al. Regeneration of K poisoned commercial SCR catalyst by acid washing[J]. Thermal power generation, 2014, 43(7): 104-109.
DOI:
PAN Siwei, CHENG Hua, WEI Zhengle, et al. Regeneration of K poisoned commercial SCR catalyst by acid washing[J]. Thermal power generation, 2014, 43(7): 104-109.DOI:
Regeneration of K poisoned commercial SCR catalyst by acid washing
The regeneration effect of acid washing on K poisoned SCR catalyst was studied.The experimental catalysts from one power plant in Guangdong province were dipped into KNO3 solution to simulate poisoning.The catalysts before and after regeneration were characterized byvarious methods.Results show that the activity of the catalyst recovered greatly after regeneration
this is partially attributed to the recovery of oxygen adsorbed in the catalyst surface.The toxic element K can be washed away effectively by acid without changing the crystal structure of the catalyst.FTIR results show that Brφnsted acid sites
which was partially recovered after regeneration
are the active chemisorbed sites for NH3 in SCR reaction.However
the stability of regenerated catalyst had declined for the decrease of acid intensity.