Performance of Fe-Ce oxide denitration catalyst and its resistance to toxicity
|更新时间:2025-09-28
|
Performance of Fe-Ce oxide denitration catalyst and its resistance to toxicity
Thermal Power GenerationVol. 45, Issue 1, Pages: 37-41(2016)
作者机构:
1. 中国计量学院计量测试工程学院
2. 浙江省环境保护科学设计研究院
作者简介:
基金信息:
DOI:
CLC:O643.36
Published:2016
稿件说明:
移动端阅览
ZHANG Guangxue, ZHOU Anqi, FAN Haiyan, et al. Performance of Fe-Ce oxide denitration catalyst and its resistance to toxicity[J]. Thermal power generation, 2016, 45(1): 37-41.
DOI:
ZHANG Guangxue, ZHOU Anqi, FAN Haiyan, et al. Performance of Fe-Ce oxide denitration catalyst and its resistance to toxicity[J]. Thermal power generation, 2016, 45(1): 37-41.DOI:
Performance of Fe-Ce oxide denitration catalyst and its resistance to toxicity
The impregnation method was employed to prepare the CeO_2-Fe_2O_3/TiO_2 catalyst and the influence of reaction temperature on denitrification efficiency of the CeO_2-Fe_2O_3/TiO_2 catalyst with different amounts of CeO_2 was studied.Moreover
the SO_2 resistance and alkali metal poisoning resistance of the10%CeO_2
3%Fe_2O_3catalysts were investigated.The experimental results show that
the optimum reaction temperature for the CeO_2-Fe_2O_3/TiO_2 catalyst is 350℃.The optimum proportion of iron cerium oxide catalyst is CeO_2 in 10%and Fe_2O_3 in 3%
with this proportion
the NO_ removal rate can reach up to 95.65%.The 10%-3%CeO_2-Fe_2O_3/TiO_2 catalyst has good performance of SO_2 resistance.The alkali metal(K
Na)salt has poisoned effect on the catalyst
but has no influence on the catalytic active ingredient of crystal phase
it just weakened the combination between the active ingredient and the carrier.The potassium salt has more significant influence than the sodium salt.The denitration performance degradation may be caused by the reduction in NH_3 adsorption ability.