Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler
|更新时间:2025-09-28
|
Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler
Thermal Power GenerationVol. 45, Issue 7, Pages: 104-109(2016)
作者机构:
1. 西安热工研究院有限公司
2. 福建省鸿山热电有限责任公司
作者简介:
基金信息:
DOI:
CLC:TK223.31
Published:2016
稿件说明:
移动端阅览
ZHOU Ke, SHE Yuanyuan, LU Fen, et al. Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler[J]. Thermal power generation, 2016, 45(7): 104-109.
DOI:
ZHOU Ke, SHE Yuanyuan, LU Fen, et al. Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler[J]. Thermal power generation, 2016, 45(7): 104-109.DOI:
Operation adjustment for high temperature corrosion in water wall of supercritical opposed firing boiler
Due to the strong reducing atmosphere and H_2S formation around the water wall of a supercritical opposed firing boiler
serious high temperature corrosion occurred in the water walls.To solve this problem
the single factor alternate method was applied to experimentally investigate the effects of main operating parameters on H_2S concentrations around side water wall.The results show that
on the basis of customary boiler operating condition
after a series of regulations
such as weakening the tertiary air swirl of the main burner appropriately
distributing the tertiary air flow as bowl type
strengthening the secondary air swirl of the main burner appropriately
increasing the swirling air ratio of the OFA burner
reducing direct air ratio of the OFA burner
increasing the running oxygen concentration appropriately
distributing the mills output uniformly
increasing the primary air velocity appropriately
and reducing the coal fineness
the H_2S concentration around the side water wall decreased from 876.5mg/m~3 to 352.2mg/m~3.The atmosphere around the water wall surface was greatly improved
and the security of the boiler operation was enhanced.